RE: precoating boron

From: John Berryman <wordguy1950_at_yahoo.com>
Date: Thu, 24 Jan 2013 15:43:59 -0700

Never worked with boron, but this discussion prompts a question:

 

Is it possible that the boron, as it is extruded (?), spun (?), or drawn
through a die (?) is coated with some sort of lubricant, and that it needs
to be degreased (detergent?, acetone?, mineral spirits?) to prevent the glue
from "beading?"

 

From: Indoor_Construction_at_yahoogroups.com
[mailto:Indoor_Construction_at_yahoogroups.com] On Behalf Of Neil Dennis
Sent: Thursday, January 24, 2013 3:25 PM
To: Indoor_Construction_at_yahoogroups.com
Subject: [Indoor_Construction] precoating boron

 

  

Mark, what would happen if you drew the boron thru a bit of fine grain
foam or maybe felt that is saturated with thin glue ?

Just a thought, wombat