crinkling stuff

From: Neil Dennis <wombatt_at_gmail.com>
Date: Mon, 25 Apr 2011 12:53:21 -0400

FWIW, I suggest "crinkling" the tissue plan sheet for the Dennydarts,
like you say, wad it up into a ball,but with the tissue you can iron it
afterward. This is to "cool down" the shrinkage that causes warps.
Wonder if that would also hold true for film ?

wombat - wadded up that blue film from the paper delivery to weigh it,
now gotta try and smooth it out.
Received on Mon Apr 25 2011 - 09:53:44 CEST