Re: Glue dilution

From: Mark F1diddler <f1diddler_at_yahoo.com>
Date: Sun, 20 Feb 2011 17:58:34 -0000

--- In Indoor_Construction_at_yahoogroups.com, themaxout@... wrote:
>
> Geoff,
>
> Another thought is the condition of the boron as a bondable surface. Has
> anyone thought about prep? How about a bit of acetone or MEK as a "wipe"
> on the material using a small soft artists brush?

For me it de rigeur to wipe down every piece of boron before use, not just swab it with a brush, but to squeeze and pull it through acetone soaked tissue. I'm sure it helps, but boron seperation is still problematic for me (and apparently others.)

My latest theory is that changing humidity is the culprit. Boron is dimensionally stable, high or low humidity, but indoor balsa is not. So the difference amounts to shear forces, given enough time.
Mark F1diddler